Author Affiliations
Abstract
1 Department of Green Energy &
2 Semiconductor Engineering, Hoseo University, Asan, South Korea
We fabricate white phosphorescent organic light-emitting diodes (PHOLEDs) with three dopants and double emissive layer (EML) to achieve color stability. The white PHOLEDs use FIrpic dopant for blue EML (B-EML), and Ir(ppy)3:Ir(piq)3 dopants for green:red EML (GR-EML) with N,N.'-dicarbazolyl-3, 5-benzene (mCP) as host material. Thicknesses of B-EML and GR-EML are adjusted to form a narrow recombination zone at two EML's interface and charge trapping happens in EML according to wide highest occupied molecular orbital and/or lowest unoccupied molecular orbital energy band gap of mCP and smaller energy band gap of dopants. The total thickness of both EMLs is fixed at 30 nm in the device structure of ITO (150 nm)/MoO3 (2 nm)/N,N'-diphenyl-N,N'-bis(l-naphthyl-phenyl)-(l,l'-biphenyl)-4, 4'-diamine (70?nm)/mCP:Firpic-8.0% (12?nm)/mCP:Ir(ppy)3-3.0%:Ir(piq)3-1.5% (18 nm)/2',2',2''-(1,3,5-benzinetriyl)-tris(1-phenyl-1-H-benzimidazole) (30 nm)/8-hydroxyquinolinolato-lithium (2 nm)/Al (120 nm). White PHOLED shows 18.25 cd/A of luminous efficiency and white color coordinates of (0.358 and 0.378) at 5000 cd/m2 and color stability with slight CIEXY change of (0.028 and 0.002) as increasing luminance from 1000 to 5000 cd/m2.
300.2140 Emission 300.6170 Spectra 330.1690 Color 230.3670 Light-emitting diodes 
Chinese Optics Letters
2014, 12(10): 102302

关于本站 Cookie 的使用提示

中国光学期刊网使用基于 cookie 的技术来更好地为您提供各项服务,点击此处了解我们的隐私策略。 如您需继续使用本网站,请您授权我们使用本地 cookie 来保存部分信息。
全站搜索
您最值得信赖的光电行业旗舰网络服务平台!